WS30W Consumables FAQs
Tip adaptors, diffusers, nozzles, necks, liners and coolant checks for a flexible-neck, liquid-cooled MIG torch.
Will turning the shielding gas up fix porosity?

Not necessarily. A maker's operating manual for this type of torch lists shielding gas flow that is too low or too high as a cause of poor shielding, because too much flow causes turbulence that mixes air into the gas. Trade guidance says the same: set the flow for the current rather than as high as it will go.
Check the other causes first: spatter inside the nozzle or in the gas discharge holes, draughts at the weld, rust, grease or moisture, a gas leak, and holding the nozzle too far from the work. Use anti-spatter sparingly, as too much can contaminate the gas. Follow the torch maker's flow guidance.
What should I check on the coolant side before I start welding?

A maker's manual for this type of torch says to check that the cooling unit is running and has enough coolant, and that the torch and interconnecting hoses are connected correctly, with the colour-coded connectors matched and no sharp bends. Keep the connectors free of dirt and metal powder, and keep an eye on the coolant level, especially with long cable sets.
Some torches have a thermal shield that stops welding if coolant flow is weak or missing. If it trips, do not carry on until the cause is found and fixed. Follow the manual for your cooler and torch.
Why does the contact tip wear, and when should I replace it?

Wire feeding through the tip gradually wears the bore, an effect often called keyholing, and spatter or arcing can damage the contact face. A worn tip can make the wire feed unevenly and the arc unstable.
A maker's troubleshooting list says to replace the contact tip when its contact face is damaged by spatter or sparking, and to check that the tip and liner suit the wire in use. A trade article advises inspecting the tip regularly and replacing it as needed, as there is no fixed interval. Also check that the tip is tight, since a loose tip adds resistance and heat.
How do I look after the front end between jobs?

The welding end of a MIG torch needs the most maintenance because of the heat and wear. A maker's manual says to remove spatter, check the insulation, contact tip and gas nozzle, replace worn or damaged parts, and check there is no spatter or dirt in the gas discharge holes.
Do not remove spatter by hitting the work with the torch, and do not use sharp tools, because scratched surfaces make spatter stick more. Apply anti-spatter compound to the front of the nozzle only. Work with the torch cool and the power source off, and replace any damaged insulation straight away.