Gas Purging Tools

Gas Purging Tools FAQs

Straight answers to the questions people ask most when choosing and using gas purging tools for TIG welding.

What is back purging and why is it needed?icon-minus-redicon-plus-red

Back purging fills the inside of a pipe or the underside of a joint with an inert gas, normally argon, while you weld from the other side. It keeps air away from the back of the weld.

Without it, the root of a weld in stainless steel and some other alloys oxidises, forming a rough, dark, sugary surface that can weaken the weld and reduce its corrosion resistance. Purging gives a smooth, clean root that is often a requirement on food, pharmaceutical and pressure pipework.

Which metals need purging?icon-minus-redicon-plus-red

It matters most for stainless steels, duplex and other high-alloy steels, titanium, and nickel alloys, where oxidation of the weld root damages corrosion resistance or the weld itself. Titanium is especially sensitive, and needs protection on both sides while it cools.

Ordinary carbon steel does not normally need it, though a purge can improve root quality. Many specifications for pipework or food and process systems require purging, so check the one that applies to your work.

What gas should I use and how much flow?icon-minus-redicon-plus-red

Argon is the usual purge gas for stainless steel and most other metals, and it is heavier than air, which helps it displace the air from the pipe. Some jobs use other inert gases or mixtures if the specification says so.

Use a regulator with a flowmeter and start with a higher flow to clear the air, then reduce to a gentle flow while welding. Too much flow creates turbulence and pressure in the pipe, which pushes on the weld pool and can spoil the root. Follow the maker's guidance for the system you use.

How long should I purge before I weld?icon-minus-redicon-plus-red

Long enough to replace the air in the enclosed space with argon, to the oxygen level your procedure or specification requires. This depends on the volume of the pipe, the gas flow and the vent size, so there is no single time that fits every job.

The most reliable check is an oxygen analyser suitable for purge-level readings, which shows the oxygen level in the purged space; some specifications require one. Where the maker or your procedure gives a purge time or number of volume changes, follow that. Colour of the first weld is only a rough guide. When in doubt, purge for longer.

What are the main types of purge system?icon-minus-redicon-plus-red

Pipe stoppers (expanding plugs) seal the ends of a pipe length. Inflatable purge bags and twin bag systems seal either side of the joint, so you purge only a small volume. Double-seal systems use two seals with a gas feed between them. Purge chambers and trailing shields protect the weld on the outside as well.

Which you choose depends on the pipe size, the number of joints and the material. Smaller purged volumes use less gas and purge faster.

When should I choose inflatable purge bags?icon-minus-redicon-plus-red

Inflatable bags are a good choice where you weld many joints on different pipe sizes, on long runs where sealing the whole pipe would waste gas, or where you can only reach one end. Each bag covers a range of pipe sizes.

They reduce the volume to purge and are reusable. They must be matched to the pipe size and kept clear of the heat of the weld, because heat can damage or burst them. Heat-resistant versions are made for jobs where the pipe stays hot.